ApplyLabWork S100 DLP Modeling Instructions

June 4, 2024
APPLYLABWORK

D75, S100, Pro95, & Pro55
DLP Modeling – Clear
(DMD-R001CR)

APPLYLABWORK PRINTING TIPS

Check:

  • UV optical pathways are clean
  • The resin tank is free of defect
  • Resin is well shaken

RayWare: [MoonRay Pinter]
Open RayWare software(version 2.8.1 and later) and connect to the printer.

Print Setup:
Select printer model
Material: SprintRay standard clear
Layer Thickness:50/100 µm

ApplyLabWork S100 DLP Modeling - app 1

  • When printing arches directly on the build platform, vertically or horizontally supports are not needed.
  • For detailed calibration for resin can refer to Dimension and Tolerance.

Washing:
IPA 95%, maximum for up to 5 minutes, gently shake off / blow off excess IPA quickly, and set print in a shaded airy place to dry completely before curing.
Extended time in IPA causes deformation. The dried print might be a little tacky to the touch.

Post-curing:

Pro-Cure: (firmware version 1.51 and later)

Select Custom, and then select the condition as30°C for 10 min.

Form Cure:
Select Custom Profile, and then select the condition as 60°C for 15 min.

Other:
Heat prints to 60°C, depending on the size, adjust time accordingly (15~40 mins). Move the warm print to the UV-curing chamber for 40 seconds. A yellow tint may appear after UV curing but will subside in a few days

Storage:
DO NOT keep the resin in the tank for more than 3 days. Filter out all debris in the case of failed print jobs

Design Concept Series

Documents / Resources

| ApplyLabWork S100 DLP Modeling [pdf] Instructions
S100 DLP Modeling, S100, DLP Modeling, Modeling
---|---

Read User Manual Online (PDF format)

Read User Manual Online (PDF format)  >>

Download This Manual (PDF format)

Download this manual  >>

Related Manuals