APPLYLABWORK PRINTING TIPS
Check
- Tank and LCD screen are clean
- Shake well (60 sec) before pouring
- Tank and platform are tightened properly
Exposure Setting Recommendation Chart
Printer| Layer Thickness (μm)| Bottom (Burn-In) Layers|
Normal Layer Exposure Time (s)| Bottom Layer Exposure Time (s)|
Rest Time After Retract (s)| Lifting Distance (mm)| Lifting Speed
(mm/min)| Retract Speed (mm/min)
---|---|---|---|---|---|---|---|---
Shuffle| 50| 6| 10| 40| 6| 5| 60| 150
100| 6| 15| 40| 6| 5| 60| 150
Shuffle XL| 50| 6| 9| 40| 8| 5| 60| 150
100| 6| 13| 40| 8| 5| 60| 150
Sonic| 50| 6| 2.5| 25| 6| 5| 60| 150
100| 6| 4.5| 25| 6| 5| 60| 150
Sonic Mini| 50| 6| 4| 25| 6| 5| 60| 150
100| 6| 6| 25| 6| 5| 60| 150
Sonic Mighty 4K| 50| 6| 3.6| 30| 8| 5| 60| 150
100| 6| 5| 30| 8| 5| 60| 150
Sonic Mighty 8K| 50| 6| 3.8| 30| 8| 5| 60| 150
100| 6| 5.2| 30| 8| 5| 60| 150
Elegoo Mars2 Pro| 50| 6| 2.6| 25| 6| 5| 60| 150
100| 6| 4| 25| 6| 5| 60| 150
Elegoo Mars3 Ultra 4K| 50| 6| 3.1| 25| 6| 5| 60| 150
100| 6| 4.2| 25| 6| 5| 60| 150
Elegoo Staurn S
| 50| 6| 3.4| 25| 8| 5| 60| 150
100| 6| 4.6| 25| 8| 5| 60| 150
Anycubic Photon MonoX| 50| 6| 1.7| 25| 8| 5| 1 (mm/s)| 2.5 (mm/s)
100| 6| 2.4| 25| 8| 5| 1 (mm/s)| 2.5 (mm/s)
Each printer is unique, light intensity varies from printer to printer, even
within same model and make. Please adjust normal exposure time from above
recommended settings ± 2 (± 0.2 ~ 0.5 for Mono LCD printer) for optimal
results.
Sizing calibration, stl file: https://www.thingiverse.com/thing:1586206
Washing
Submerge print in clean IPA (95+% concentration) for up to 5 minutes, gently shake-off/blow-off excess IPA, set prints in shaded, airy place to dry before post-curing. Extended time in IPA causes deformation.
Post Curing
Curing Chamber | Temperature (℃) | Time (min) |
---|---|---|
Form cure (Formlabs) | 60 | 60 |
Phrozen cure XL (Phrozen) | – | 60 |
Mercury x Cure (Elegoo) | – | 60 |
For optimal material performance, 405 nm light of total energy per unit area
required: 18000 mJ/cm².
Example: light power or curing chamber: 5 mW/cm² (higher power per unit
area shortens curing time), 18000 (mJ) / 5 (mW) / 60 (sec) = 60 mins of curing
time.
Storage
- Keep resin in shaded environment; temperature between 15℃ and 26℃
- NOT accessible to children
- Filter used resin before storage
- To extend tank life, limit prolong storing resin in tank
Notes: Slight pigment settlement is normal. Gently mix remaining resin in
resin tank with soft wiper for color evenness. Ensure there are no pigment
settled on the resin tank bottom before start printing.
In the case of failed/incomplete print, filter used resin to ensure there are
no debris in the reins before next print.
Prototype Engineering Series
Documents / Resources
|
ApplyLabWork MPT-RI001DO MSLA Dusty
Olive
[pdf] User Guide
MPT-RI001DO MSLA Dusty Olive, MPT-RI001DO, MSLA Dusty Olive, Dusty Olive,
Olive
---|---
References
Read User Manual Online (PDF format)
Read User Manual Online (PDF format) >>