eurofins MG-1012 Medium Wood Slat Walls Owner’s Manual
- June 1, 2024
- eurofins
Table of Contents
eurofins MG-1012 Medium Wood Slat Walls
TEST REPORT
Photographs
Annexure A
Classification Requirement as per IBC.
Correction Factor
CORRECTION FACTOR FOR CALCULATING FLAME SPREAD INDEX
- If this total area (At) is less than or equal to 97.5 ft-min then
- The flame spread index shall be FSI = 0.515* A.
- If the total area (Ar) is greater than 97.5 ft-min then
- The flame spread index shall be FSI = 4900/ (195 – A).
- Here At represents Total Area i.e. AT = A1 + A2
- A1 = Area Under the curve where the first peak is observed.
- A2 = Area just above the curve in the line of the First peak point.
CORRECTION FACTOR FOR CALCULATING SMOKE DEVELOPED INDEX
Smoke Developed (SD) is determined by dividing the total area under the obscuration curve by that of the cement board and multiplying by 100. SD is then rounded to the nearest multiple of 5 if less than 200. SD values over 200 are rounded to the nearest multiple of 50. Smoke Developed Index = Area under the Obscuration Curve × 100 The area under the Red Oak Curve
Discipline: Mechanical
Group: Building Materials
TEST REPORT FOR DETERMINING THE FLAME SPREAD INDEX AND SMOKE DEVELOPED INDEX
Test Sponsor
SHINIL FRAME CO.LTD
Product Name
POLYSTYRENE WALL PANELS WITH GYPSUM BOARD (Name given by test sponsor)
Test Standards:
ASTM E84-2021; Standard Test Method for Surface Burning Characteristics of
Building Materials.
Testing Laboratory
Spectro Analytical Labs Pvt. Ltd.
S-1 GNEPIP, Surajpur Industrial Area
Kasna, Greater Noida, Phase – V
Gautam Budha Nagar (U.P.)
Pin Code: 201308
Ph: 0120-2341251/52
Specimen Verification
length: 600mmm
Thickness: 19mm
Sample Preparation
The sample was in sheet form having dimensions 19 mm in thickness 600 mm in
width and 1000 mm in length. Some sheets were used to spread over the tunnel
to form the requisite specimen length. During testing the sample was self-
supporting.